- Compare
- Scotch Chrome 1000 vs Agfachrome 1000 RS
Film comparison
3M Scotch Chrome 1000 vs Agfa-Gevaert Agfachrome 1000 RS
What the catalogue holds about each, and the times they share. A dash means a figure has not been read off a datasheet — nothing here is estimated.
Specification side by side
| Film |
3M Scotch Chrome 1000
|
Agfa-Gevaert Agfachrome 1000 RS
|
|---|---|---|
| Maker | 3M | Agfa-Gevaert |
| ISO | 1000 | 1000 |
| Type | Colour reversal | Colour reversal |
| Process | E-6 | E-6 |
| Status | Discontinued | Discontinued (1995) |
| Formats | — | — |
| Grain (RMS) | — | — |
| Resolving power | — | — |
| Latitude | — | — |
| First released | — | 1984 |
| Reciprocity data | No | No |
| Published times | 4 | 4 |
Developers in common
Each film’s time at its own box speed in the same developer, at the same dilution and temperature. Every time opens the full table for that film in that developer.
| Dilution · °C | Scotch Chrome 1000 EI 1000 | Agfachrome 1000 RS EI 1000 |
|---|---|---|
| working solution · 38 °C | 6:15 | 6:15 |