- Compare
- Kolorit 125 Tungsten vs A-Color 125
Film comparison
KONO! Kolorit 125 Tungsten vs SFL A-Color 125
What the catalogue holds about each, and the times they share. A dash means a figure has not been read off a datasheet — nothing here is estimated.
Specification side by side
| Film |
KONO! Kolorit 125 Tungsten
|
SFL A-Color 125
|
|---|---|---|
| Maker | KONO! | SFL |
| ISO | 125 | 125 |
| Type | Colour negative | Colour negative |
| Process | C-41 | C-41 |
| Status | In production | In production |
| Formats | — | — |
| Grain (RMS) | — | — |
| Resolving power | — | — |
| Latitude | — | — |
| First released | — | — |
| Reciprocity data | No | No |
| Published times | 12 | 12 |
Developers in common
Each film’s time at its own box speed in the same developer, at the same dilution and temperature. Every time opens the full table for that film in that developer.
| Dilution · °C | Kolorit 125 Tungsten EI 125 | A-Color 125 EI 125 |
|---|---|---|
| working solution · 30 °C | 8:00 | 8:00 |
| working solution · 38 °C | 3:15 | 3:15 |
| Dilution · °C | Kolorit 125 Tungsten EI 125 | A-Color 125 EI 125 |
|---|---|---|
| working solution · 22 °C | 50:00 | 50:00 |
| working solution · 24 °C | 35:00 | 35:00 |
| working solution · 27 °C | 21:00 | 21:00 |
| working solution · 29.5 °C | 13:00 | 13:00 |
| working solution · 32 °C | 8:30 | 8:30 |
| working solution · 35 °C | 5:45 | 5:45 |
| working solution · 39 °C | 3:30 | 3:30 |
| Dilution · °C | Kolorit 125 Tungsten EI 125 | A-Color 125 EI 125 |
|---|---|---|
| working solution · 38 °C | 3:00 | 3:00 |
| working solution · 39 °C | 3:30 | 3:30 |
| Dilution · °C | Kolorit 125 Tungsten EI 125 | A-Color 125 EI 125 |
|---|---|---|
| working solution · 38 °C | 3:15 | 3:15 |