Specification side by side
| Film |
SFL A-Color 125
|
KONO! Kolorit 125 Tungsten
|
|---|---|---|
| Maker | SFL | KONO! |
| ISO | 125 | 125 |
| Type | Colour negative | Colour negative |
| Process | C-41 | C-41 |
| Status | In production | In production |
| Formats | — | — |
| Grain (RMS) | — | — |
| Resolving power | — | — |
| Latitude | — | — |
| First released | — | — |
| Reciprocity data | No | No |
| Published times | 12 | 12 |
Developers in common
Each film’s time at its own box speed in the same developer, at the same dilution and temperature. Every time opens the full table for that film in that developer.
| Dilution · °C | A-Color 125 EI 125 | Kolorit 125 Tungsten EI 125 |
|---|---|---|
| working solution · 30 °C | 8:00 | 8:00 |
| working solution · 38 °C | 3:15 | 3:15 |
| Dilution · °C | A-Color 125 EI 125 | Kolorit 125 Tungsten EI 125 |
|---|---|---|
| working solution · 22 °C | 50:00 | 50:00 |
| working solution · 24 °C | 35:00 | 35:00 |
| working solution · 27 °C | 21:00 | 21:00 |
| working solution · 29.5 °C | 13:00 | 13:00 |
| working solution · 32 °C | 8:30 | 8:30 |
| working solution · 35 °C | 5:45 | 5:45 |
| working solution · 39 °C | 3:30 | 3:30 |
| Dilution · °C | A-Color 125 EI 125 | Kolorit 125 Tungsten EI 125 |
|---|---|---|
| working solution · 38 °C | 3:00 | 3:00 |
| working solution · 39 °C | 3:30 | 3:30 |
| Dilution · °C | A-Color 125 EI 125 | Kolorit 125 Tungsten EI 125 |
|---|---|---|
| working solution · 38 °C | 3:15 | 3:15 |